Author
Listed:
- Hongxin Yang
(Shenzhen University)
- Yuan Zhang
(Clear Water Bay
Shenzhen University)
- Zhipeng Liu
(Shenzhen University)
- Chunfang Hu
(Shenzhen University)
- Junbiao Li
(Shenzhen University)
- Hailong Liao
(Shenzhen University)
- Minhua Shao
(Clear Water Bay
The Hong Kong University of Science and Technology)
- Meng Ni
(The Hong Kong Polytechnic University)
- Bin Chen
(Shenzhen University)
- Zongping Shao
(Curtin University)
- Heping Xie
(Shenzhen University)
Abstract
Thermo-mechanics of cathode is closely related to the durability of high-temperature solid oxide fuel cells (SOFCs), with two main mechanical failures during thermal cycling: interface delamination and bulk cracking of cathode. Bulk cracking, caused by insufficient fracture strength/stiffness is a big concern but often overlooked. Here, we introduce chemical hydration to offset the thermal expansion, enhancing the cathodic mechanical stiffness and fracture strength, thus promoting the thermo-mechanical durability of cathode in proton ceramic fuel cells (PCFCs). Such chemical-induced expansion offset is achieved by strengthening intergranular bonding inside the bulk cathode after the hydration, preventing granule detachment during thermal shrinkage. As a demonstration, the stiffness-enhanced air electrode (BaCo0.7Ce0.15Y0.15O3, noted as s-BCC-Y) exhibits 86% enhancement of fracture strength, thus thermal cycling stability with almost no degradation after 35 harsh thermal cycles between 600 and 300 °C, surpassing pristine BaCo0.7Ce0.3O3 and many cobalt-free PCFC cathodes. Benefitted from the improved stiffness of cathode, full cell with the s-BCC-Y electrode demonstrates enhanced power output. This work highlights the importance of bulk cathode thermo-mechanics in developing robust SOFCs for high temperature energy applications.
Suggested Citation
Hongxin Yang & Yuan Zhang & Zhipeng Liu & Chunfang Hu & Junbiao Li & Hailong Liao & Minhua Shao & Meng Ni & Bin Chen & Zongping Shao & Heping Xie, 2025.
"Hydration-induced stiffness enabling robust thermal cycling of high temperature fuel cells cathode,"
Nature Communications, Nature, vol. 16(1), pages 1-12, December.
Handle:
RePEc:nat:natcom:v:16:y:2025:i:1:d:10.1038_s41467-025-57611-1
DOI: 10.1038/s41467-025-57611-1
Download full text from publisher
Corrections
All material on this site has been provided by the respective publishers and authors. You can help correct errors and omissions. When requesting a correction, please mention this item's handle: RePEc:nat:natcom:v:16:y:2025:i:1:d:10.1038_s41467-025-57611-1. See general information about how to correct material in RePEc.
If you have authored this item and are not yet registered with RePEc, we encourage you to do it here. This allows to link your profile to this item. It also allows you to accept potential citations to this item that we are uncertain about.
We have no bibliographic references for this item. You can help adding them by using this form .
If you know of missing items citing this one, you can help us creating those links by adding the relevant references in the same way as above, for each refering item. If you are a registered author of this item, you may also want to check the "citations" tab in your RePEc Author Service profile, as there may be some citations waiting for confirmation.
For technical questions regarding this item, or to correct its authors, title, abstract, bibliographic or download information, contact: Sonal Shukla or Springer Nature Abstracting and Indexing (email available below). General contact details of provider: http://www.nature.com .
Please note that corrections may take a couple of weeks to filter through
the various RePEc services.